Polymer Property : Density = 1.4 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.4 g/cc
0.051 lb/in³
ASTM D792
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade
Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica..