Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.364 g/cc | 0.04928 lb/in³ | ISO 1183 |
Lanxess Pocan® TS 3220 901510 PBT + PET, 20% Glass Fiber PBT+PET, 20% glass fibers, injection molding, impact modified, low tendency to warp, improved surface finish |