Polymer Property : Density = 1.309 g/cc
Polymer Property :
Density =
1.309 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
1.309
g/cc
0.04729
lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP QF006 PA 6/10
LNP THERMOCOMP* QF006 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber.