Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.295 g/cc | 0.04678 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF004 PA 66 LNP THERMOCOMP* RF004 is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
Density | 1.295 g/cc | 0.04678 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66 LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber. |