Polymer Property : Density = 1.229 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.229 g/cc
0.04440 lb/in³
ASTM D792
Multibase Multi-Flex® TPE A 7020 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.