Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.225 g/cc | 0.04426 lb/in³ | ISO 1183 |
Stir SpA C 2053 64 AT (PVC) Application: Molding for superior thermal inner soleInformation provided by STIR SpA |
|||
Density | 1.225 g/cc | 0.04426 lb/in³ | ISO 1183 |
Stir SpA C 2053 68 AT (PVC) Application: Molding for superior thermal inner soleInformation provided by STIR SpA |
|||
Density | 1.225 g/cc | 0.04426 lb/in³ | ISO 1872-2/ISO 1183 |
Borealis Casico™ FR6082 Reduced Fire Hazard Jacketing Compound Casico™ FR6082 is a thermoplastic, reduced fire hazard, zero halogen black jacketing compound combined with high mechanical strength, toughness and excellent extrusion properties. It is based on th.. |