Physical Properties Metric English Comments
Density 1.218 g/cc
0.04400 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® 943AR PC (Asia Pacific)
Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors.
Density 1.218 g/cc
0.04400 lb/in³
ISO 1183
Stir SpA T 4099 A (PVC)
Application: Non-toxic transparent pipe for conveying waterInformation provided by STIR SpA