Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.214 g/cc | 0.04386 lb/in³ | ISO 1183 |
Stir SpA SG 55 ATC (PVC) Application: Extrusion non-toxic seal for wood window and door framesInformation provided by STIR SpA |
|||
Density | 1.214 g/cc | 0.04386 lb/in³ | |
Dow ISONATE™ 143L Modified MDI ISONATE™ 143L modified MDI is a polycarbodiimide-modified diphenylmethane diisocyanate.Information provided by Dow |
|||
Density | 1.214 g/cc | 0.04386 lb/in³ | |
Dow ISONATE™ 143L Modified MDI ISONATE™ 143 is a polycarbodiimide-modified diphenylmethane diisocyanate. Liquid at room temperature, this product has a low viscosity and good storage stability down to 75°F. The polycarbodiimi.. |