Physical Properties Metric English Comments
Density 1.194 g/cc
0.04314 lb/in³
Dow Nordel® IP 4725P Dense Extrusion
FormulationNordel® IP 4725P
Density 1.194 g/cc
0.04314 lb/in³
BASF Triphenylphosphine Pellets
Formula: C18H15PCAS: 603-35-0Description: Triphenyl phosphine pellets are a colorless solid, and have a faint specific odor. It is insoluble with water. Synonyms: TPP, Triphenylphosphane, Triphenyl..
Density 1.194 g/cc
0.04314 lb/in³
BASF Triphenylphosphine Molten
Formula: C18H15PCAS: 603-35-0Description: Triphenyl phosphine pellets are a colorless solid, and have a faint specific odor. It is insoluble with water.Synonyms: TPP, Triphenylphosphane, Triphenylp..