Polymer Property : Density = 1.165 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.165 g/cc
0.04209 lb/in³
ASTM D792
Multibase Multi-Flex® TPE A 4410 NAT
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Density 1.165 g/cc
0.04209 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON AX00756 ABS
LNP STAT-KON* AX00756 is a compound based on ABS resin containing Stainless Steel. Added feature of this material is: Electrically Conductive.