Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.145 - 1.155 g/cc | 0.04137 - 0.04173 lb/in³ | |
Solvay GLOKILL® PQ Surfactant Description: Cationic polymer based on quaternary ammonium.Identification: POLYQUATERNARY AMMONIUM CHLORIDE AQUEOUS SOLUTIONAvailable in: Asia Pacific, Europe, Latin America and North AmericaStabili.. |