Polymer Property : Density = 1.133 g/cc
Polymer Property :
Density =
1.133 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
1.133
g/cc
0.04093
lb/in³
ISO 1183
Lanxess Durethan® DP A 32 901510 Nylon 66
PA 66 standard injection molding grade, non-reinforced, very easy release