Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.097 g/cc | 0.03963 lb/in³ | |
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite Processed by selective laser sintering (SLS). Windform® XT 2.0 is the evolution of the ground breaking high performance Windform® XT, the carbon fiber reinforced composite material, known for its.. |