Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.092 g/cc | 0.03945 lb/in³ | ASTM D 792 |
Shakespeare Isocorâ„¢ TT25TI Nylon 6 Terpolymer Isocorâ„¢ is a low viscosity nylon terpolymer. Isocorâ„¢ TT25TI is useful as an additive for improved impact in phenolics, polyesters, urethanes and nylons. The unique chemistry affords it.. |
|||
Density | 1.092 g/cc | 0.03945 lb/in³ | ISO 1183 |
Denka TE-10 Transparent Resin Polymer (MABS resin) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |