Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.039 g/cc | 0.03754 lb/in³ | ASTM D792 |
North Wood Plastics Polypropylene with 40% Wood Fiber, Molding Grade Data provided by North Wood Plastics, Inc. |
|||
Density | 1.039 g/cc | 0.03754 lb/in³ | ASTM D 792 |
Shakespeare Isocorâ„¢ HG20SC Nylon 612 Isocorâ„¢ HG20SC us a medium viscosity compounding grad PA-612 based nylon. This resin is specifically suited for applications requiring lower moisture regain and greater dimensional stability... |
|||
Density | 1.039 g/cc | 0.03754 lb/in³ | ASTM D 792 |
Shakespeare Isocorâ„¢ HG26SI medium viscosity PA-612 Isocorâ„¢ HG26SI is a medium viscosity PA-612 based nylon. This resin is specifically suited for applications requiring low moisture regain and greater dimensional stability. Isocorâ„¢ HG2.. |