Polymer Property : Density = 1.032 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.032 g/cc
0.03728 lb/in³
NEU NeuSoft™ 596-60A Medical Ether TPU / SBC blend
Density 1.032 g/cc
0.03726 lb/in³
Calculated from weight of 17 oz/sy
Mid-Mountain Materials ARMATEX® SF22 Silicone Rubber Coated Glass Fabric
Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based...
Density 1.032 g/cc
0.03728 lb/in³
Struktol STRUKSILON 8030 Silicone Stabilizer for PU-Rigid Foam
STRUKSILON 8030 is a universal stabilizer for the production of polyurethane rigid foams. Due to its excellent flow properties and the very good insulation values that can be achieved STRUKSILON 803..