Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.993 - 1.007 g/cc | 0.0359 - 0.03638 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GE 4960 BR HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |