Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.9525 g/cc | 0.03441 lb/in³ | ASTM D792 |
Dow DGDA-2475 NT High Density Polyethylene Resin DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in corrugated pipe applications. It has been specifically designed for extrusion of corrugated pipes with the.. |