Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.941 - 0.947 g/cc | 0.0340 - 0.0342 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 7746 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.941 - 0.947 g/cc | 0.0340 - 0.0342 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 7746 A HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.932 - 0.947 g/cc | 0.0337 - 0.0342 lb/in³ | Average value: 0.937 g/cc Grade Count:35 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |