Polymer Property : Density = 0.9035 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.9035 g/cc
0.03264 lb/in³
ASTM D792
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP)
AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In..