Physical Properties Metric English Comments
Density 0.828 - 0.871 g/cc

@Temperature 15.0 °C
0.0299 - 0.0315 lb/in³

@Temperature 59.0 °F
Unipetrol Light Stabilized Oil Hydrogenate
Stabilized oil hydrogenates are a fraction boiling above approximately 250°C, obtained from crude oil through distillation and mild hydrocracking. They are a mixture of light colour hydrocarbons of..
Density 0.835 - 0.871 g/cc

@Temperature 15.0 °C
0.0302 - 0.0315 lb/in³

@Temperature 59.0 °F
Unipetrol Medium Stabilized Oil Hydrogenate
Stabilized oil hydrogenates are a fraction boiling above approximately 250°C, obtained from crude oil through distillation and mild hydrocracking. They are a mixture of light colour hydrocarbons of..