Polymer Property : Density = 0.829 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.805 - 0.829 g/cc
0.0291 - 0.0299 lb/in³
Lord Adhesives HPC-5C Hydrogenated Nitrile Butadiene Rubber Coating
LORD HPC-5B and HPC-5C are one-part, room temperature curing HNBR coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fluid and ozone resista..