Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.824 g/cc @Temperature 15.0 °C |
0.0298 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Exxsol™ D140 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.824 g/cc @Temperature 15.6 °C |
0.0298 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn™ 5 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |