Physical Properties Metric English Comments
Density 0.8088 - 0.8328 g/cc
0.02922 - 0.03009 lb/in³
Lord Adhesives Chemlok® Y-1520A Adhesive
LORD Chemlok® Y-1520A adhesive is a clear, one-coat adhesive used to bond specialty elastomers to metal and plastics during vulcanization of the rubber. Chemlok Y-1520A adhesive is useful for bon..