Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.798 g/cc @Temperature 15.6 °C |
0.0288 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn™ 2C Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Density | 0.798 g/cc @Temperature 15.6 °C |
0.0288 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn™ 2 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |