Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 21.6 g/cc | 0.780 lb/in³ | |
Wieland 1951 Wilaform Platinum Platinum alloy for technical use.Applications: casting, chains, laminar decoration, pipes, tubingDental |
|||
Density | 21.6 g/cc | 0.780 lb/in³ | |
CMW® ELKONIUM 32 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |