Polymer Property : Density = 0.743 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.743 g/cc

@Temperature 15.0 °C
0.0268 lb/in³

@Temperature 59.0 °F
ISO 12185
ExxonMobil Exxsol™ DSP100/140 Dearomatized Fluid
Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil