Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.6669 g/cc | 0.02409 lb/in³ | |
DayGlo GloPrill Hyperdispersed Colorant GloPrill is a high-performance fluorescent colorant developed especially for polyolefins. Designed with the plastics concentrate/masterbatch producer in mind, these supercharged colorants develop br.. |