Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.631 g/cc @Temperature 15.0 °C |
0.0228 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Exxsol™ Pentane 100 S Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.631 g/cc @Temperature 15.0 °C |
0.0228 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Exxsol™ Pentane 80 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |