Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.582 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 16.1 - 16.7 g/cc
0.582 - 0.603 lb/in³
H.C. Starck WCu 85/15 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
Density 16.1 g/cc
0.582 lb/in³
Wieland 1916 Wilaform Gold
Hard palladium white gold alloy with beautiful grey color.Applications: casting, chains, laminar decoration, pipes, tubingDental