Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 15.4 - 15.8 g/cc | 0.556 - 0.571 lb/in³ | |
MarkeTech W80Cu Tungsten/Copper Heat Sink Material WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c.. |