Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.529 - 0.560 g/cc | 0.0191 - 0.0202 lb/in³ | Dried |
Pyrotek Pyrocast L-40 Insulating Refractory Pyrocast L-40 is a fiber free refractory moldable designed for use in contact with molten aluminum. L-40 has excellent workability for use as an insulating lining or patching material.Recommended C.. |