Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 15.2 g/cc | 0.549 lb/in³ | |
PSM Industries PolyAlloys MIM-WC-6Co Tungsten Carbide Information Provided by PolyAlloys, a division of PSM Industries |
|||
Density | 15.2 - 15.6 g/cc | 0.549 - 0.564 lb/in³ | |
MarkeTech WCu20 Tungsten Copper Alloy Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Density | 15.2 g/cc | 0.549 lb/in³ | |
China Tungsten YG3 Tungsten Carbide for Cutting Tools Wear resistance less than YG3X only, sensitive to impact and vibration for continuous semi-finish and finish turning of castiron, non-ferrous metals and their alloys and for finish turning of thread.. |
|||
Density | 15.2 g/cc | 0.549 lb/in³ | |
China Tungsten YG3X Tungsten Carbide for Cutting Tools Best wear resistance among W-Co alloys yet impact toughness comparatively low, High speed finishing of small chip section of cast irons, non-ferrous metals & alloys quenched steel and alloy steel.In.. |