Polymer Property : Density = 0.5361 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 14.84 g/cc
0.5361 lb/in³
CMW® ELKONITE® 10W3 Copper Tungsten RWMA Class 11
Electrical contacts resistant to arcing, power transformer switches, resistance / projection welding electrodes, and EDM electrodesInformation provided by CMW Inc.
Density 14.84 g/cc
0.5361 lb/in³
CMW® THERMKON® 83 Tungsten Copper parts
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.