Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 14.81 g/cc | 0.5350 lb/in³ | |
Williams Advanced Alloys WS305 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |