Polymer Property : Density = 0.5220 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 14.45 g/cc
0.5220 lb/in³
China Tungsten YG10X Tungsten Carbide
Information provided by China Tungsten
Density 14.45 g/cc
0.5220 lb/in³
China Tungsten YG11 Tungsten Carbide
Information provided by China Tungsten
Density 14.45 - 14.65 g/cc
0.5220 - 0.5293 lb/in³
China Tungsten Z25 Tungsten Carbide for Mining Purposes
Of high toughness and wear resistance as well as good versatility, for rotary hammer rock drill bits and pillar bit drills, for f14~f16 medium hard and hard rock formations.Information provided by C..