Physical Properties Metric English Comments
Density 12.5 - 13.5 g/cc
0.452 - 0.488 lb/in³
China Tungsten YWR2 Tungsten Carbide with Rare Earth Additive
Higher wear resistance and service strength than YW2 capable of undergoing high impact load. For roughing and Semi-finishing of heat resistant steel ,hi-Mn steel, stainless steel and high alloy stee..
Density 12.5 g/cc
0.452 lb/in³
CMW® ELKONITE® 1W3 Copper Tungsten RWMA Class 10
Uses: Arcing and current carrying electrical contacts. Resistance/projection welding electrodes.Information provided by CMW Inc.