Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.449 g/cc | 0.0162 lb/in³ | ASTM D3574 |
Rogers Corporation Bisco™ HT-840 Cellular Silicone Foam Extra firm grade silicone sponge. UL recognized of flame retardance.Applications: High closure-force gaskets, Press-pads where conformable imprinting support is required, such as decal lamination o.. |
|||
Density | 0.449 g/cc | 0.0162 lb/in³ | |
Pyrotek I-28 Insulating Board Pyrotek's I-28 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-28 also contains no RCF's.A.. |
|||
Density | 0.449 - 0.513 g/cc | 0.0162 - 0.0185 lb/in³ | |
Engineered Syntactic Systems BZ-30 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |
|||
Density | 0.449 g/cc | 0.0162 lb/in³ | |
Trelleborg AEM Eccofloat® TG-28/4000 Syntactic Foam TG Grade syntactic foams are lightweight and economical for building manned and remote operating vehicles. The foams are also used to manufacture mine neutralization systems because of their zero ma.. |