Polymer Property : Density = 0.4433 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 12.27 g/cc
0.4433 lb/in³
CMW® ELKONITE® G13 Tungsten Carbide Silver contact material ASTM 663, Class B, infiltrated
For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc.