Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.400 - 0.440 g/cc | 0.0145 - 0.0159 lb/in³ | ISO 845-88 |
Eurofoam Siliconcell 411/PLT Platinic Silicone Foam Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |