Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 12.1 g/cc | 0.437 lb/in³ | |
Wieland 1007 Wilaform Gold Silver white gold alloy for all kinds of decoration manufacturing.Applications: casting, chains, coin/shape, laminar decoration, tubingDental |