Polymer Property : Density = 0.430 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.430 - 0.490 g/cc
0.0155 - 0.0177 lb/in³
True, 3M QCM 14.24.6
3M HGS6000 Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Density 0.430 - 0.490 g/cc
0.0155 - 0.0177 lb/in³
3M iM16K Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.430 - 0.490 g/cc
0.0155 - 0.0177 lb/in³
3M K46 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..