Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 11.64 g/cc
0.4205 lb/in³
CMW® ELKONITE® TC10 Tungsten Carbide Copper material
For wiping and arcing electrical contacts and projection welding tips.Information provided by CMW Inc.
Density 11.64 g/cc
0.4205 lb/in³
Cadi 10TC Tungsten Carbide Copper
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.