Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 11.1 g/cc | 0.400 lb/in³ | |
Conforma Clad WC 219 Tungsten Carbide-Nickel Cladding Conforma Clad is a targeted wear solution applied to vulnerable surfaces of a component. The wear protection is delivered via a proprietary cloth or slurry, ranging from 0.020" to 0.120" thick.If a.. |