Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.320 - 0.380 g/cc | 0.0116 - 0.0137 lb/in³ | ISO 1183 |
Fainplast Compounds EVAtech 801S Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Density | 0.320 - 0.380 g/cc | 0.0116 - 0.0137 lb/in³ | ISO 1183 |
Fainplast Compounds EVAtech 803S Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Density | 0.320 - 0.380 g/cc | 0.0116 - 0.0137 lb/in³ | True, 3M QCM 14.24.6 |
3M HGS3000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Density | 0.320 - 0.380 g/cc | 0.0116 - 0.0137 lb/in³ | |
3M S35 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |