Polymer Property : Density = 0.373 g/cc
Polymer Property :
Density =
0.373 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
0.373
g/cc
0.0135
lb/in³
Pyrotek S-2 Fabric
Coarse fabric with low air permeability. Excellent mechanical strength and abrasion resistance.Information provided by Pyrotek.