Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 10.31 g/cc | 0.3725 lb/in³ | |
Williams Advanced Alloys C118 Solder Williams extensive offering of Contact Alloys are cast and fabricated to meet the exacting standards of various micro electronics applications. All Williams electrical contact alloys are available i.. |