Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 10.17 g/cc | 0.3674 lb/in³ | |
CMW® D54F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3 For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc. |
|||
Density | 10.17 g/cc | 0.3674 lb/in³ | |
CMW® D54X Post-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3 For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc. |