Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 10.0 g/cc
0.361 lb/in³
Lucas-Milhaupt BRAZE 716 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 716 is a nickel modified silver copper eutectic filler metal. The addition of nickel renders this alloy somewhat more sluggish in flow characteristics than the eutectic comp..
Density 10.0 g/cc
0.361 lb/in³
Lucas-Milhaupt BRAZE 716 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 716 is a nickel modified silver copper eutectic filler metal. The addition of nickel renders this alloy somewhat more sluggish in flow characteristics than the eutectic comp..
Density 10.0 g/cc
0.361 lb/in³
ASTM D792
Techmer ES HiFill® TPU 1000
Availability: North AmericaForms: PelletsFeatures: High DensityAppearance: BlackInformation provided by TP Composites, Inc.
Density 10.0 g/cc
0.361 lb/in³
Williams Advanced Alloys C106 Solder
Williams extensive offering of Contact Alloys are cast and fabricated to meet the exacting standards of various micro electronics applications. All Williams electrical contact alloys are available i..
Density 10.0 g/cc
0.361 lb/in³
CMW® ELKONIUM 1 silver, copper, nickel alloy
Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a..