Polymer Property : Density = 0.360 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 9.96 g/cc
0.360 lb/in³
Indium Corp. Indalloy 145 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Density 9.97 g/cc
0.360 lb/in³
Indium Corp. Indalloy 48 Bismuth Solder Alloy
Information Provided by Indium Corporation
Density 9.97 g/cc
0.360 lb/in³
Indium Corp. Indalloy® 10 Pb-In Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
Density 9.96 g/cc
0.360 lb/in³
Lucas-Milhaupt BRAZE 720 Silver Based Cadmium Free Filler Metal
Characteristics:Brazing 720 is the silver-copper eutectic composition and in melting it acts like a metallic element, i.e. it melts completely at a single temperature, thus it will quickly flow into..
Density 9.96 g/cc
0.360 lb/in³
Lucas-Milhaupt BRAZE 721 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal
Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc..
Density 9.96 g/cc
0.360 lb/in³
Lucas-Milhaupt BRAZE 721 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal
Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc..
Density 9.96 g/cc
0.360 lb/in³
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi..
Density 9.96 g/cc
0.360 lb/in³
Lucas-Milhaupt Silvaloy® B72 Brazing Alloy
Silvaloy B72 is the eutectic composition of the silver-copper system. It is suitable for use in controlled atmosphere brazing without the use of a paste flux. When molten, it is very fluid and may f..
Density 9.97 g/cc
0.360 lb/in³
Williams Advanced Alloys WS264 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys